Title of Invention

A METHOD AND APPARATUS FOR CLEANING A SEMICONDUCTOR SUBSTRATE

Abstract Not only can the substrate be cleaned uniformly and stably,but also a resource saving and a reduction in the waste amount can be achived. In the cleaning treatment of a substrate using an aqueous soulation of ammonium fluoride or mixture of an aqueous solution of ammonium fluoride and hydrofluoric acid as a cleaning liquid,the cleaning liquid is replenished by at least one selected from water ,ammonia,aqueous ammonia,and an aqueous soulation of ammonium fluroridde with the lapse of time during the use of the cleaning liquid.In this case,the requried amount of the liquid to be added according to the time lapse is calcuated based on the measurement date and controlled.Alternatively,the component concentration of the cleaning liquid is detected and the liquid is added according to the obtained result.
Full Text FORM 2
THE PATENTS ACT 1970
[39 OF 1970]
THE PATENTS RULES, 2003 COMPLETE SPECIFICATION
[See Section 10; rule 13]
"A METHOD AND APPARATUS FOR CLEANING A SEMICONDUCTOR
SUBSTRATE"
We, SONY CORPORATION, a Japanese company, of 7-35, Kitashinagawa 6-chome, Shinagawa-ku, Tokyo, Japan,
The following specification particularly describes the invention and
the manner in which it is to be performed:


ORIGINAL
629/MUMNP/01

GRANTED
21-9-06
04-10-01

The present invention relates to a method and apparatus for "cleaning a semiconductor substrate.
The present document is based on Japanese Priority Documents JP 2000-214974, filed in the Japanese Patent Office on July 14, 2000 and JP 2000-240134 filed on August 8, 2000 the entire contents of which being incorporated herein by reference.
BACKGROUND OF THE INVENTION
1. Field of the Invention
The present invention relates to a substrate cleaning method and a substrate cleaning apparatus for cleaning a substrate, which use, as a cleaning liquid, an aqueous solution of ammonium fluoride or a mixture of an aqueous solution of ammonium fluoride and hydrofluoric acid. More particularly, the present invention is concerned with a novel substrate cleaning method and a novel substrate cleaning apparatus, which are developed for achieving both uniform and stable cleaning treatment and reduction in the amount of the cleaning liquid used.
2. Description of the Related Art
An aqueous solution of ammonium fluoride (including arbitrary mixtures of hydrofluoric acid and ammonia, and ones containing a surfactant) is widely used in the form of a mixture thereof with hydrofluoric acid and the like for cleaning or etching a semiconductor (mainly a silicon

oxide film) substrate or a glass substrate in the production process for semiconductor or liquid crystal display (LCD).
In addition to the above example of substrate cleaning, in Unexamined Japanese Patent Application Laid-Open Specification No. 2000-150447, a mixture of ammonia and""hydrogen peroxide is used for cleaning silicon wafers. This prior art document discloses that the ammonia concentration and hydrogen peroxide concentration of the mixture are individually monitored during the cleaning, and the change with time of the chemical liquid concentration is accurately estimated based oh the results of measurements to calculate and adjust the amount of the chemical liquid to be added, so that the chemical liquid concentration is kept constant.
In these fields, for achieving reduction in weight and downsizing of products and the lowering of consumed electric power, development of a microfabrication technology for a higher integration degree is desired.
In any case of cleaning substrates using, as a cleaning liquid, for example, an aqueous solution of ammonium fluoride, a mixture of an aqueous solution of ammonium fluoride and hydrofluoric acid as mentioned above, or other chemical liquids, a higher accuracy treatment is desired.
By the way, in the above-mentioned cleaning or etching, the chemical component content, such as ammonium fluoride (NH4F), and hydrogen fluoride (HF), and moisture content of the cleaning liquid change (evaporate) with the lapse of time. Therefore, such cleaning or etching has a problem in that the etching rate for a silicon

oxide film or a glass substrate changes (increases).
This is caused by the gradual increase in the hydrofluoric acid component concentration of the cleaning liquid with the lapse of time during the use of the cleaning liquid, and the problem of the change in the concentrations of the components in the cleaning liquid has been conventionally solved by frequently replacing the cleaning liquid.
However, in this method, a great amount of the cleaning liquid is required. Especially a cleaning liquid containing ammonium fluoride is used in an ammonium fluoride concentration as high as several tens % (for example, about 40 % by weight), and hence, the amount of the chemical consumed per liquid replacement in this cleaning liquid is large, as compared to those in other cleaning liquids generally used in a chemical concentration of about several %. Accordingly, the amounts of the ammonium fluoride and hydrofluoric acid used (cost for chemicals) are to increase.
Further, after the cleaning liquid is used, a waste water treatment shown in Fig. 1 is needed, and, in this treatment, a large amount of resource (waste water treatment agent) is consumed, resulting in a large amount of waste products (waste water and sludge)(see Fig. 2).
Fig. 1 is an explanatory view illustrating a process for treating the effluent of a cleaning liquid. Effluent produced in a cleaning bath 11 is transferred to a pH-adjusting bath 12, and neutralized in this bath by, for example, a 20 % aqueous solution of calcium hydroxide. Next, the effluent is transferred to a coagulo-sedimentation bath 13 and subjected to coagulation and

sedimentation by a chemical, such as aluminum sulfate, and then, in a flocculation bath 14, is flocculated by a polymeric flocculant, such as a polyacrylamide flocculant, and subjected to sedimentation, followed by discharge in the form of sewage and sludge.
In the above treatment process, as shown in Fig. 2, for treating 1 kg of a 40 % aqueous solution of ammonium fluoride, 2.0 kg of 20 % calcium hydroxide, 0.3 kg of 8 % aluminum sulfate, and 1.6 kg of a polymeric flocculant are required, so that 2.6 kg of sludge having a solids content of 70 % and 2.3 kg of sewage waste water are produced.
In recent years, concern about the environmental problems is growing worldwide, and a demand for removing the environmental burden caused by the production of substrates for semiconductor and LCD is being increasing. Therefore, with respect to the cleaning liquid for the substrates, not only for reducing the cost, but also for achieving preservation of the environment, i.e., a saving of resource, a reduction in waste, and environmental cleaning, a solution of the problem about the reduction in the amount of the cleaning liquid used is socially desired strongly.
SUMMARY OF THE INVENTION According to the present invention, there is
provided a substrate cleaning method and a substrate
cleaning apparatus which enable a resource saving and a
reduction in waste to be achieved..
The present invention also provides a substrate
cleaning method which is developed for achieving both the

uniform and stable cleaning treatment and the reduction
in the amount of the cleaning liquid used.
Furthermore, the present invention provides a substrate cleaning apparatus which is developed for achieving both uniform and stable cleaning treatment and reduction in the amount of the cleaning liquid used.
Still furthermore, a substrate cleaning method and a substrate cleaning apparatus, which use"an aqueous solution of ammonium fluoride or a mixture of an aqueous solution of ammonium fluoride and hydrofluoric acid as a cleaning liquid is also provided according to the present invention.
According to the present invention there is provided a method for cleaning a semiconductor substrate with a thermally oxidized film or a glass used for liquid crystal display; using a cleaning liquid comprising at least one selected from the group consisting of an aqueous solution of ammonium fluoride, and a mixture of an aqueous solution of ammonium fluoride and hydrofluoric acid, comprising the steps of:
- dipping and cleaning the substrate in said cleaning liquid;
- adding a replenishing liquid, comprising at least one selected from the group consisting of water, ammonia, aqueous ammonia and an aqueous solution of ammonium fluoride with lapse of time during cleaning treatment, at a constant rate for keeping the concentration of hydrogen fluoride (HF) component constant,
wherein a temperature of the cleaning liquid is 25°C;
wherein the cleaning liquid has a composition such that the NH4F (40%): HF (50%) ratio is 400:1 and HF concentration is between 2.94 wt% to 3.04 wt%. such that the etching rate is kept constant.

According to the present invention there is also provided an apparatus for cleaning a semiconductor substrate, comprising: a substrate cleaning bath containing therein a substrate cleaning liquid comprising at least one liquid selected from the group consisting of an aqueous solution of ammonium fluoride, and a mixture of an aqueous solution of ammonium fluoride and hydrofluoric acid; and liquid feeding means for feeding a liquid comprising at least one selected from the group consisting of water, ammonia, aqueous ammonia and an aqueous solution of ammonium fluoride, and
further comprising: measuring means for measuring characteristics of
said cleaning liquid in said substrate cleaning bath; and control means
for arithmetically processing a signal from said measuring means to
control the feeding of the liquid from said liquid feeding means to
substrate cleaning bath. A nAk,vlKlr
BRIEF DESCRIPTION OF THEADRAWINGS
The above and other objects, features and advantages of the present invention will become more apparent from the following description of the presently preferred exemplary embodiments of the invention taken in conjunction with the accompanying drawings, in which:
Fig. 1 is an explanatory view illustrating a process for treating an effluent of a cleaning liquid, which is the related art.
Fig. 2 is a diagram showing a resource (chemicals) required for an effluent treatment for a cleaning liquid, which is the related art.
Fig. 3 is a graph showing the relationship between time and etching rate with respect to the cleaning liquid.
Fig. 4 is a graph showing the relationship between the time and the HF concentration of the cleaning liquid.
Fig. 5 is a diagrammatic view showing an example of a substrate cleaning.apparatus, which is .a first

embodiment of the present invention.
Fig. 6 is a graph showing the change in the HF concentration by addition of water according to the present invention.
Fig. 7 is a graph showing the change in the etching rate by addition of water according to the present invention.
Fig. 8 is a graph showing the state of controlling the etching rate and the HF concentration by addition of water according to the present invention.
Fig. 9 is a diagrammatic view showing a substrate cleaning apparatus, which is a second embodiment of the present invention.
Fig. 10 is a diagrammatic view showing an example of a substrate cleaning apparatus in which an aqueous ammonia storage tank is provided, which is a third embodiment of the present invention.
Fig. 11 is a diagrammatic view showing an example of a substrate cleaning apparatus in which an aqueous ammonia storage tank is provided, which is a fourth embodiment of the present invention.
DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS Hereinbelow, a substrate cleaning method and a substrate cleaning apparatus according to the present invention will be described in detail with reference to the accompanying drawings.
In the present invention, in the cleaning (or etching) treatment of a substrate using, as a treatment liquid (or a cleaning liquid), an aqueous solution of ammonium fluoride or a mixture of an aqueous solution of

ammonium fluoride and hydrofluoric acid, the cleaning liquid is replenished by at least one liquid selected from the group consisting of water, ammonia, aqueous ammonia, and an aqueous solution of ammonium fluoride according to the accumulative time for using the cleaning liquid and the individual component concentrations of the cleaning liquid.
Fig. 3 shows the relationship between the lapse of time and the etching rate for a thermal oxide film with respect to the mixture of ammonium fluoride and hydrofluoric acid. The cleaning liquid has a composition such that the NH4F (40 %):HF (50 %) ratio is 400:1, and the temperature of the cleaning liquid is 25° C and the thermal oxide film is comprised of Si02.
In the graph shown in Fig. 3, the time is taken as the abscissa and represented by a unit of "days", and the etching rate for a substrate is taken as the ordinate and represented by a unit of the etching rate per minute, i.e., "A/min". The etching rate changes with time as follows: after a lapse of 0 day, the etching rate is about 34 A/min; after a lapse of 11 days, the etching rate is 70 A/min; and after a lapse of 22 days, the etching rate is 95 A/ min.
As can be seen from Fig. 1, the etching rate for the thermal oxide film remarkably increases with the lapse of time.
As mentioned above, in the cleaning treatment of a substrate using the above-mentioned cleaning liquid, the etching rate changes with time, and there is a very good correlation (proportionality relation) between the etching rate and the time. This means that the moisture

content and chemical component (such as ammonium fluoride (NH4F) and hydrogen fluoride (HF)) contents of the cleaning liquid change (evaporate) with the lapse of time, and specifically means that the water component and ammonia component of the cleaning liquid evaporate at a constant rate, so that the concentration of the hydrogen fluoride (HF) component (which directly contributes to the etching for the thermal oxide film) in the cleaning liquid increases at a constant rate.
Fig. 4 shows the change in the HF concentration of the cleaning liquid with the lapse of time.
The time is taken as the abscissa and represented by a unit of "days", and ranges from 0 to 25 days. On the other hand, the HF concentration of the mixture is taken as the ordinate and represented by a unit of "% by weight (wt%)", and ranges from 0 to 0.6 wt% and is shown in a scale of 0.1 wt%.
After a lapse of 0 day, the HF concentration is 0.1 wt%; after a lapse of 11 days, the HF concentration is 0.35 wt%; and after a lapse of 22 days, the HF concentration is 4.7 wt%.
From the above, it is found that the HF concentration of the mixture increases at a constant rate with the lapse of time.
Thus, in the cleaning (etching) treatment of a substrate using an aqueous solution of ammonium fluoride or a mixture of an aqueous solution of ammonium fluoride and hydrofluoric acid, the HF concentration of the cleaning liquid is required to be kept constant. In this case, a most effective method is the one in which water that readily evaporates from the cleaning liquid is

appropriately added to .the„cleaning liquid.
Specifically, when water is added to the cleaning liquid with the lapse of time, a rise in the HF concentration can be suppressed, so that the etching rate can be kept constant. Also when an aqueous solution of ammonium fluoride is added to the cleaning liquid, the HF concentration is lowered, so that a similar effect can be expected.
On the other hand, when ammonia is added to the cleaning liquid, HF in the cleaning liquid is neutralized by ammonia to form ammonium fluoride, so that a rise in the HF concentration of the cleaning liquid can be suppressed. When aqueous ammonia is added, both the dilution effect and the neutralization effect can be expected.
By the above-mentioned method, not only can the yield of substrates for semiconductor and liquid crystal be improved, but also the frequency of the liquid replacement can be reduced, thus making it possibleto achieve both the saving of chemicals, such as the cleaning liquid and waste water treatment agent, and the reduction in sludge and waste water amount.
Fig. 5 shows an example of the construction of the substrate cleaning apparatus according to the present invention.
This substrate cleaning apparatus comprises a substrate treatment bath 21 for storing therein a cleaning liquid comprising, for example, a mixture of ammonium fluoride and hydrofluoric acid, and for subjecting a substrate to cleaning treatment, and a circulation pump 22 for circulating the cleaning liquid

which is the overflow back to the substrate treatment bath 21. For example, a substrate, which is a substance to be treated, is accommodated in a substrate carrier and dipped in the cleaning liquid in the substrate treatment bath 21, and thus performing a cleaning (etching) treatment.
The characteristic feature of the above apparatus resides in that the substrate treatment" bath 21 is provided with a constant delivery pump 23 and a controller 24, by which feeding water and addition of water through the pump 23 is controlled.
As mentioned above, the HF component concentration of the cleaning liquid increases with the lapse of time at a constant rate, so that the etching rate for the thermal oxide film remarkably increases.
Therefore, in this substrate cleaning apparatus, the HF concentration is controlled by the controller 24 so as to be kept constant by adding water to the substrate treatment bath 21 with the lapse of time by means of the constant delivery pump 23 so that the etching rate is kept substantially constant.
Fig. 6 shows the change in the HF concentration when water is added. In this graph, the time is taken as the abscissa and represented by a unit of "hours (hrs)", and ranges from 0 to 300 hrs. On the other hand, the HF concentration is taken as the ordinate and represented by a unit of "wt%", and ranges from 2.92 to 3.06 wt%. After a lapse of 0 hr, the HF concentration is 2.94 wt%; and after a lapse of 220 hrs, the HF concentration is 3.04 wt%. When water is added at this point in time, the HF concentration is lowered to 2.95 wt%. After a lapse of

further about 20 hrs, the HF concentration slightly increases to 2.96 wt%.
As apparent from the above description, the HF concentration which increases with the lapse of time goes back to the original concentration by addition of water. The control of the HF concentration by addition of water leads to the control of the etching rate, and, as shown in Fig. 7, the etching rate is also lowered by the addition of water.
With respect to the amount of the water added and the timing of the water addition, data is obtained as shown in Fig. 3 and Fig. 4 to calculate the amount of the water which evaporates with the lapse of time, making it possible to introduce the optimal amount of the water added and the optimal conditions for the timing of the water addition.
Fig. 7 is a graph showing the state of controlling the etching rate and HF concentration by addition of water.
The time is taken as the abscissa and represented by a unit of "hours (hrs)", and ranges from 0 to 250 hours. On the other hand, the etching rate is taken as the ordinate and represented by a unit of "nm/min", and ranges from 65 to 85 nm/min.
After a lapse of 25 hours, the etching rate is 74 nm/min; after a lapse of 70 hours, the etching rate is 76 nm/min; and after a lapse of 220 hours, the etching rate is 82 nm/min. When water is added at a point in time after 220 hours, the etching rate is lowered to about 72 nm/min.
Thus, the etching rate and the HF concentration can

be kept in a constant range by intermittently adding water.
A graph showing the relationship between the etching rate and the hydrofluoric acid concentration when water is intermittently added is illustrated in Fig. 8.
Fig. 8 shows an example in which water is intermittently added, but the conditions for water addition may be any of continuous addition and intermittent addition. For keeping the concentration constant, the continuous addition is preferred.
In the above substrate cleaning apparatus, the timing of the addition of water is controlled based on the measurement data, but, as shown in Fig. 9, a concentration measuring unit 35 can be provided to measure the concentration of the cleaning liquid being circulated, so that the addition of water can be controlled based on the concentration data in real time.
Specifically, the concentrations of the components (e.g., ammonia, hydrofluoric acid, and water) in the cleaning liquid are individually measured by means of the concentration measuring unit 35, and the measurement result is transmitted to a controller 34 comprised of a computer and a central monitoring unit to determine the addition and calculate the required amount of addition, followed by transmission of an instruction for replenishment to a water feeding line (constant delivery pump 33). Then, whether or not the addition is made in accordance with the instruction is confirmed by a measurement by means of the concentration measuring unit 35.
In the present invention, as a method for measuring

the concentrations of the components in the cleaning liquid, a measurement of an absorbance at a predetermined wavelength, an infrared absorption spectrum, an ultraviolet absorption spectrum, an index of refraction, a specific gravity, a transmittance, or an electric conductivity may be performed and a measuring unit, such as a Karl Fischer moisture titrator or liquid (ion) chromatography may be used.
Fig. 10 and Fig. 11 show an example in which an aqueous ammonia storage tank 47 or 57 for feeding aqueous ammonia is provided instead of the constant delivery pump 23 or 33 for feeding water in Fig. 5 and Fig. 9, respectively.
By adding aqueous ammonia instead of water, the HF concentration is effectively controlled, so that the etching rate is controlled to be kept constant.
In the feeding of ammonia, not only aqueous ammonia but also other appropriate aqueous solutions can be used, and further, ammonia gas can also be used. Alternatively, an aqueous solution of ammonium fluoride can be used, and ammonium fluoride can be used in combination with ammonia.
As mentioned above, by adding to the cleaning liquid water, aqueous ammonia, or an aqueous solution of ammonium fluoride in consideration of the etching rate and the individual component concentrations of the cleaning liquid at a certain point in time in the treatment, the etching treatment by the cleaning liquid can be conducted uniformly and stably (namely, the etching rate for an oxide film can be kept constant), so that there is no need to frequently replace the cleaning liquid differing from the conventional cleaning.

Therefore, the life time of the cleaning liquid can be prolonged, and the reduction in frequency of the liquid replacement contributes to a reduction in the cleaning liquid consumed (resource saving) and a reduction in the waste water treatment agent required for the waste water treatment of the cleaning liquid (resource saving). Further, the reduction in these chemicals used contributes to a reduction in the amount of sludge and waste water produced upon the waste water treatment (reduction in the amount of waste).
Thus, the present invention not only achieves the uniform and stable substrate treatment but also contributes to resource saving and the reduction in the amount of waste, namely, preservation of the environment.
As mentioned above, by using the method and apparatus of the present invention, in the cleaning of a substrate using an aqueous solution of ammonium fluoride or a mixture of an aqueous solution of ammonium fluoride and hydrofluoric acid, not only can the treatment be conducted uniformly and stably, but also the frequency of replacement of the cleaning liquid can be reduced, thus making it possible to achieve the saving of resource, i.e., chemicals (a cleaning liquid and a waste water treatment agent), and considerably reduce the amount of sludge and waste water produced upon the treatment.
Although the invention has been described in its preferred form with a certain degree of particularity, obviously many changes and variations are possible therein. It is therefore to be understood that the present invention may be practiced otherwise than as

We Claim:
1. A method for cleaning a semiconductor substrate with a
thermally oxidized film or a glass used for liquid crystal display; using
a cleaning liquid comprising at least one selected from the group
consisting of an aqueous solution of ammonium fluoride, and a
mixture of an aqueous solution of ammonium fluoride and
hydrofluoric acid, comprising the steps of:
- dipping and cleaning the substrate in said cleaning liquid;
- adding a replenishing liquid, comprising at least one selected from the group consisting of water, ammonia, aqueous ammonia and an aqueous solution of ammonium fluoride with lapse of time during cleaning treatment, at a constant rate for keeping the concentration of hydrogen fluoride (HF) component constant,
wherein a temperature of the cleaning liquid is 25°C; wherein the cleaning liquid has a composition such that the NH4F (40%): HF (50%) ratio is 400:1 and HF concentration is between 2.94 wt% to 3.04 wt%. such that the etching rate is kept constant.
2. The method as claimed in claim 1, further comprising the step
of measuring characteristics of said cleaning liquid, wherein a kind
and an amount of said replenishing liquid are determined in response
to a result of the measurement of said cleaning liquid.

3. The method as claimed in claim 2, wherein, in the measuring step, hydrofluoric acid concentration is measured at a predetermined time interval and water is fed as said replenishing liquid so that a measurement value of said concentration falls within a predetermined range.
4. The method as claimed in claim 2, wherein said characteristics of said cleaning liquid is measured by at least one measurement selected from the group consisting of measurements of an absorbance at a predetermined wavelength, an infrared absorption spectrum, an ultraviolet absorption spectrum, an index of refraction, a specific gravity, a transmittance and an electric conductivity, a measurement by means of a moisture titrator, and a measurement by means of liquid (ion) chromatography.
5. The method as claimed in claim 3, wherein said hydrofluoric acid concentration of said cleaning liquid is measured by at least one measurement selected fn?m the group consisting of measurements of an absorbance at a predetermined wavelength, an infrared absorption spectrum, an ultraviolet absorption spectrum, an index of refraction, a specific gravity, a transmittance, and an electric conductivity, a measurement by means c?f a moisture titrator, and a measurement by means of liquid (ion) chromatography.

6. An apparatus for cleaning a semiconductor substrate,
comprising: a substrate cleaning bath containing therein a substrate
cleaning liquid comprising at least one liquid selected from the group
consisting of an aqueous solution of ammonium fluoride, and a
mixture of an aqueous solution of ammonium fluoride and
hydrofluoric acid; and liquid feeding means for feeding a liquid
comprising at least one selected from the group consisting of water,
ammonia, aqueous ammonia and an aqueous solution of ammonium
fluoride, and
further comprising: measuring means for measuring characteristics of said cleaning liquid in said substrate cleaning bath; and control means for arithmetically processing a signal from said measuring means to control the feeding of the liquid from said liquid feeding means to substrate cleaning bath.
7. The apparatus as claimed in claim 6 wherein said measuring means comprises means for measuring at least one wavelength characteristic selected from the group consisting of an absorbance at a predetermined wavelength, an infrared absorption spectrum, an ultraviolet absorption spectrum and an index of refraction.
8. The apparatus as claimed in claim 6, wherein said measuring means comprises means for measuring at least one physical value selected from the group consisting of a specific gravity and a transmittance.

9. The apparatus as claimed in claim 6, wherein said measuring means comprises means for measuring an electric conductivity.
10. The apparatus as claimed in claim 6, wherein said measuring means comprises at least one measurement means selected from the group consisting of a moisture titrator and liquid (ion) chromatography.
11. A method for cleaning a semiconductor substrate substantially as herein described with reference to the accompanying drawings.
12. An apparatus for cleaning a semiconductor substrate substantially as herein described with reference to the accompanying drawings.
Dated this the 5th day of July, 2001
[JAYANTA PAL]
Of Remfry & Sagar
Attorney for the Applicants

Documents:


Patent Number 204624
Indian Patent Application Number 629/MUM/2001
PG Journal Number 24/2007
Publication Date 15-Jun-2007
Grant Date 28-Feb-2007
Date of Filing 05-Jul-2001
Name of Patentee SONY CORPORATION
Applicant Address of 7-35,Kitashinagawa 6-chome, Shinagawa-ku, Tokyo,Japan.
Inventors:
# Inventor's Name Inventor's Address
1 YOSHIHIRO FUJITANI c/o Sony Corporation of 7-35,Kitashinagawa 6-chome, Shinagawa-ku, Tokyo,Japan
2 YASUHITO INAGAKI c/o Sony Corporation of 7-35,Kitashinagawa 6-chome, Shinagawa-ku, Tokyo,Japan.
3 MINEO SHIMIZU c/o Sony Corporation of 7-35,Kitashinagawa 6-chome, Shinagawa-ku, Tokyo,Japan
PCT International Classification Number H 01 L 21/00
PCT International Application Number N/A
PCT International Filing date
PCT Conventions:
# PCT Application Number Date of Convention Priority Country
1 P2000-214974 2000-07-14 Japan